박사

Study on crack-sealing of cement composite via encapsulating the granulated healing material

이용수 2015년
논문상세정보
    • 저자 이용수
    • 형태사항 26 cm: xi, 162 p. :: 삽도 ;
    • 일반주기 권두 Abstract, 권말 국문요지 수록, 지도교수: 유재석, 참고문헌: p. 152-159
    • 학위논문사항 건축환경공학과,, 한양대학교 대학원 :, 2015. 8, 학위논문(박사)-
    • 발행지 서울
    • 언어 eng
    • 출판년 2015
    • 발행사항 한양대학교 대학원,
    • 주제어 건축환경공학
    유사주제 논문( 13)
' Study on crack-sealing of cement composite via encapsulating the granulated healing material' 의 주제별 논문영향력
논문영향력 선정 방법
논문영향력 요약
주제
  • 건축환경공학
동일주제 총논문수 논문피인용 총횟수 주제별 논문영향력의 평균
14 0

0.0%

' Study on crack-sealing of cement composite via encapsulating the granulated healing material' 의 참고문헌

  • Yang JH, Lee YM, Kim YI, Experimental Pharmaceutics. Shinil, Korea, 2007. p.268-277.
  • Wu M., Johannesson B, Geiker M, A review: self-healing in cementitious materials andengineered cementitious composite as a self-healing material, Construction andBuilding Materials 2012; 28(1): 571-83.
  • Wright J, In: Pumps/osmotic-ruminal osmotic bolus: In Encyclopediaof Controlled DrugDelivery, Vol. 2, E. Mathiowitz (Ed.): Wiley; 1999. p. 915-920.
  • Wagh MA, Dilip KP, Salunkhel KS, Chavan NV, Daga VD, Techniques used in orallydisintegrating drug delivery system, International Journal of Drug Delivery 2010; 2(2),98-107.
  • Van Tittelboom K, Gruyaert E, Rahier H, De Belie N, Influence of mix composition onthe extent of autogenous crack healing by continued hydration or calcium carbonateformation, Construction and Building Materials 2012; 37: 349-359.
  • Van Tittelboom K, De Belie N, Van Loo D, Jacobs P, Self-healing efficiency ofcementitious materials containing tubular capsules filled with healing agent, Cementand Concrete Composites 2011; 33(4): 497-505.
  • Ukrainczyk N, Matusinovic T, Thermal properties of hydrating calcium aluminate cementpastes, Cement and Concrete Research 2010; 40(1): 128-36.
  • Tousey MD, The Granulation Process 101 Basic Technologies for Tablet Making,Pharmaceutical Technology 2002; 8-13.
  • Tittelboom KV, Belie ND, Muynck WD, Verstraete W. Use of bacteria to repair cracksin concrete. Cem Concr Res 2010;40:157?166.
  • Thao TDP, Johnson TJS, Tong QS, Dai PS, Implementation of self-healing in concrete?proof of concept. The IES J Part A: Civil Struct Eng 2009; 2(2): 116?125.
  • Stuckrath C, Serpell R, Valenzuela LM, Lopez M, Quantification of chemical andbiological calcium carbonate precipitation: Performance of self-healing in reinforcedmortar containing chemical admixtures, Cement and Concrete Composites 2014; 50:10-5.
  • Song IH, An Experimental Study on the Use of Recycled Concrete Fine Aggregate inSelf-Consolidating Concrete(SCC), Thesis for the degree of master, HanyangUniversity, 2009. p. 14-25.
  • Sisomphon K, Copuroglu,O, Koenders EAB, Self-healing of surface crack in mortarswith expansive additive and crystalline additive, Cement and Concrete Composites2012; 34(4): 566-74.
  • Sisomphon K, Copuroglu O, Koenders EAB, Effect of exposure conditions on selfhealing behavior of strain hardening cementitious composites incorporating variouscementitious materials, Construction and Building Materials 2013; 42: 217-24.
  • Silva DA, Monteiro PJM, Early Formation of Ettringite in Tricalcium Aluminate?CalciumHydroxide?Gypsum Dispersions. Journal of the American Ceramic Society, 2007; 90(2):614-617.
  • Shangraw RF, DA. Demarest, A survey of current industrial practices in the formulationof tablets and capsules, Pharm Tech, 1993. p. 32-44.
  • Schmitt HC, Effect of clinker composition of setting and early strength of cement.Zem-Kalk-Gips, 1973; 26(2): 63-66.
  • Sandler N, Lammens RF, Pneumatic dry granulation: potential to improve rollercompaction technology in drug manufacture, Expert Opinion on Drug Delivery 2011;8(2): 225-36.
  • Sakai Y, Fukuta T. Experimental study on enhancement of self-restoration of concretebeams using SMA wire. In: Proceedings of smart structures and materials 2003: smartsystem and nondestructive evaluation for civil infrastructures, San Diego, CA, USA;2003.
  • Ryou JS, Yang NW, Lee YS, A Study on Properties of Retarder via Tabletting Method,Journal of the Korea Concrete Institute, 2013; 25(2): 201-207.
  • Ryou JS, Lee YS, Use of tabletting & coating accelerator for the prevention ofearly-frost of concrete in cold weather, Cold Regions Science and Technology 2013;87: 1?5.
  • Ryou JS, Lee YS, Properties of early-stage concrete with setting-accelerating tablet incold weather, Materials Science and Engineering A 2012; 532: 84?90.
  • Ryou JS, Lee YS, A Study on Setting Time and Early Strength of Tablet-ShapedAccelerators, Journal of the Korea Concrete Institute, 2011; 23(3): 347-352.
  • Ruotsalainen M, Heinamaki J, Guo H, Laitinen N, Yliruusi J, A novel technique forimaging film coating defects in the film-core interface and surface of coated tablets.European journal of pharmaceutics and biopharmaceutics, 2003; 56(3): 381-388.
  • Ravve A, In: Principles of Polymer Chemistry: Plenum Press; 2003. p. 269-339.
  • Prime RB, Bair HE, Vyazovkin S, Gallagher PK, Riga A, Thermogravimetric analysis(TGA). Thermal Analysis of Polymers: Fundamentals and Applications, 2009. p.241-317.
  • Peppas NA, Hydrogels and drug delivery. Current Opinion in Colloid & InterfaceScience, 1997: 2(5): 531-537.
  • Park CJ, Koh KT, Han MC, Han CG, Analysis of Drying Shrinkage of the ConcreteUsing Calcium Sulfa Aluminate (CSA) Based Expansive Additive, Applied Mechanicsand Materials 2012; 121: 2445-2250.
  • Pang JWC, Bond IP. Bleeding composites ?damage detection and self-repair using abiomimetic approach. Composites Part A 2005; 36: 183?188.
  • Pang JWC, Bond IP. A hollow fibre reinforced polymer composite encompassingself-healing and enhanced damage visibility. Compos Sci Technol 2005; 65: 1791?1799.
  • Ohtsu M, Damage evaluation in freezing and thawing test of concrete by elastic-wavemethods, Materials and Structures 2011; 44(10): 1725-1734.
  • Neville A, Autogenous healing - a concrete miracle, Concrete International 2002;24(11): 76-82.
  • Naik TR, Malhotra VM, Popovics JS, The ultrasonic pulse velocity method, CRChandbook on nondestructive testing of concrete 1, 1991. p. 1-31.
  • Moon HY, Kim HS, Choi DS, Relationship between average pore diameter and chloridediffusivity in various concretes. Construction and Building Materials, 2006; 20(9):725-732.
  • Mindess S, Young JF, Darwin D, In: Concrete; second ed.: Prentice Hall; 2002. p.193?220.
  • Mehta PK, Monteiro PJM, Concrete - Microstructure, Properties, and Materials, thirded. Mc Graw Hill, USA, 2006. p. 135-148.
  • Malhotra VM, Carino NJ, Handbook on nondestructive testing of concrete, secondedition, ASTM International, CRC press, USA, 2004. Chapter 8Malhotra VM, Testing hardened concrete: Nondestructive methods, ACI/IOWA stateuniversity press, USA, 2004. p. 74-102.
  • METHOCEL as a granulation binding agent for immediate release tablet and capsuleproducts. Wilmington, DE, Dow Chemical, 1996. p. 15-17.
  • Li VC, Herbert E, Robust self-healing concrete for sustainable infrastructure, Journalof Advanced Concrete Technology 2012; 10:207-218.
  • Lee YS, Ryou JS, Self healing behavior for crack closing of expansive agent viagranulation/film coating method. Construction and Building Materials, 2014: 71:188-193.
  • Lee YS, Ryou JS, A Characteristics of Fly-ash Concrete Incorporating Tablet-shapedAccelerators in Cold Weather, Journal of the Recycled Construction Resources, 2014;2(1): 40-45.
  • Lee YS, Lim DS, Chun BS, Ryou JS, Characterization of a sodium aluminate(NaAlO2)-based accelerator made via a tablet processing method. Journal of CeramicProcessing Research, 2013; 14(1): 87-91.
  • Lee YS, A fundamental study on the properties of concrete using by tablet ofaccelerators, Thesis for the degree of master, Hanyang University, 2011. p. 22-25.
  • Lee JD, Nondestructive analysis of concrete structures, IlKwang books, Korea, 2011.p.47.
  • Kwon JW, Min SH, Rhee SH, Kim YB, Studies on the Tablet Product Design : Effectsof Anhydrous Lactose and Corn Starch on the Preparation of Prednisolone Tablet byDirect Compression Method, Journal of the Pharmaceutical society of korea, 1976:20(2): 63-69.
  • Kumar SA, Santhanam M, (2006, December). Detection of Concrete Damage UsingUltrasonic Pulse Velocity Method. In National Seminar on Non-Destructive Evaluation,India, 2006. p. 301-308.
  • Korsmeyer RW, Gurny R, Doelker E, Buri P, Peppas NA, Mechanisms of solute releasefrom porous hydrophilic polymers, International journal of Pharmaceutics 1983; 15(1):25-35.
  • Kim YS, Concrete crack control, Kimoondang, Korea, 2010. p. 12-49.
  • Kim YB, Mathematical Optimization Techniques in Drug Product Design and ProcessAnalysis. Optimization Techniques in Tablet Design, Journal of the Pharmaceuticalsociety of korea, 1974: 18(1): 49-58.
  • KCI, Korea Concrete Standard Specification, Korea Concrete Institute, 2009. p.170-175.
  • Joseph C, Jefferson AD, Isaacs B, Lark R, Gardner D. Experimental investigation ofadhesive-based self-healing of cementitious materials. Mag Concr Res 2010; 62(11):831?833.
  • Jefferson A, Joseph C, Lark R, et al. A new system for crack closure of cementitiousmaterials using shrinkable polymers. Cem Concr Res 2010; 40: 795?801.
  • Jaroenratanapirom D, Sahamitmongkol R, Self-crack closing ability of mortar withdifferent additives, Journal of Metals, Materials and Minerals 2011; 21(1): 9-17.
  • Jacobsen S, Marchand J, Boisvert L, Effect of cracking and healing on chloridetransport in OPC concrete, Cement and Concrete Research 1996; 26(6): 869-881.
  • Igarashi S, Kunieda M, Nishiwaki T, Research activity of JCI technical committeeTC-075B: Autogenous healing in cementitious materials. In Proceedings of 4thInternational Conference on Construction Materials: Performance, Innovations andStructural Implications, Con Mat, Nagoya, Japan, August 2009.
  • Heinamaki J, Ruotsalainen M, Lehtola VM, Antikainen O, Yliruusi J, Optimization ofaqueous-based film coating of tablets performed by a side-vented pan-coatingsystem. Pharmaceutical development and technology, 1997; 2(4): 357-364.
  • Hearn N, Self-sealing, autogenous healing and continued hydration: What is thedifference, Materials and Structures 1998; 31(8): 563-567.
  • Gun Sul Do Seo editorial, Concrete cracks and measures, Gun Sul Do Seo, Korea,2005. p. 29-109.
  • Edvardsen C, Water permeability and autogenous healing of cracks in concrete. ACIMater J 1999; 96: 448?454.
  • Dale EW, Air-suspension technique of coating drug particles.-A preliminary report.Journal of the American Pharmaceutical Association. 1959; 48(8): 451-454.
  • Coolepardi M, Baldini G, Pauri M, Retardation of tricalcium aluminate hydration bycalcium sulfate Journal of the American Ceramic Society, 1979: 62(1-2): 33-36.
  • Atahan HN, Carlos C, Chae S, Monteiro PJM, Bastacky J, The morphology ofentrained air voids in hardened cement paste generated with different anionicsurfactants. Cement and Concrete Composites, 2008; 30(7): 566-575.
  • Arai Y, Cement Materials Chemistry, second ed. Chonnam National University Press,Korea, 1998. p. 156-252.
  • Allen RTL, Edwards SC, Shaw JDN, Repair of concrete structures. CRC Press, USA,1992. p. 13-23.
  • Allen LV, Popovich NG, In: Ansel’s Pharmaceutical Dosage Forms and Drug DeliverySystems: Lippincott Williams & Wilkins; 2005. p. 83?125.
  • Ahn TH, Kishi T. The effect of geomaterials on the autogenous healing behavior ofcracked concrete. In: Proceeding of 2nd ICCRRR, Cape Town, South Africa; 2008. p.235?240.
  • Ahn TH, Kishi T, Crack self-healing behavior of cementitious composites incorporatingvarious mineral admixtures, Journal of Advanced Concrete Technology 2010; 8(2):171-186.