2-Body Wear Comparison of Monolithic Zirconia Crown, Gold Crown and Enamel against Zirconia : 지르코니아에 대한 법랑질과 금관 및 단일체 지르코니아관의 2-body 마모비교

권민석 2015년
논문상세정보
' 2-Body Wear Comparison of Monolithic Zirconia Crown, Gold Crown and Enamel against Zirconia : 지르코니아에 대한 법랑질과 금관 및 단일체 지르코니아관의 2-body 마모비교' 의 주제별 논문영향력
논문영향력 선정 방법
논문영향력 요약
주제
  • enamel
  • fixed partial dentures
  • wear
  • zirconia
동일주제 총논문수 논문피인용 총횟수 주제별 논문영향력의 평균
192 0

0.0%

' 2-Body Wear Comparison of Monolithic Zirconia Crown, Gold Crown and Enamel against Zirconia : 지르코니아에 대한 법랑질과 금관 및 단일체 지르코니아관의 2-body 마모비교' 의 참고문헌

  • Wang L, Liu Y, Si W, Feng H, Tao Y, Ma Z. Friction and wearbehaviors of dental ceramics against natural tooth enamel. J Eur CeramSoc 2012;32:2599-606.
  • Van Der Bilt A, Tekamp A, Van Der Glas H, Abbink J. Bite forceand electromyograpy during maximum unilateral and bilateral clenching.25Eur J Oral Sci 2008;116:217-22.
  • Tinschert J, Natt G, Mautsch W, Augthun M, Spiekermann H. Fractureresistance of lithium disilicate-, alumina-, and zirconia-based three-unitfixed partial dentures: a laboratory study. Int J Prosthodont2001;14:231-8.
  • Stober T, Bermejo J, Rammelsberg P, Schmitter M. Enamel wearcaused by monolithic zirconia crowns after 6 months of clinical use. JOral Rehabil 2014;41:314-22.
  • Serra C, Manns A. Bite force measurements with hard and soft bitesurfaces. J Oral Rehabil 2013;40:563-8.
  • Seghi RR, Rosenstiel SF, Bauer P. Abrasion of human enamel bydifferent dental ceramics in vitro. J Dent Res 1991;70:221-5.
  • Sailer I, Gottner J, Kanel S, Franz Hammerle CH. Randomizedcontrolled clinical trial of zirconia-ceramic and metal-ceramic posteriorfixed dental prostheses: a 3-year follow-up. Int J Prosthodont2009;22:553-60.
  • Sabrah AH, Cook NB, Luangruangrong P, Hara AT, Bottino MC.Full-contour Y-TZP ceramic surface roughness effect on synthetichydroxyapatite wear. Dent Mater 2013;29:666-73.
  • Raigrodski AJ. Contemporary materials and technologies for all-ceramicfixed partial dentures: a review of the literature. J Prosthet Dent2004;92:557-62.
  • Piconi C, Maccauro G. Zirconia as a ceramic biomaterial. Biomaterials1999;20:1-25.
  • Owais AI, Shaweesh M, Abu Alhaija ES. Maximum occusal biteforce for children in different dentition stages. Eur J Orthod2013;35:427-433.
  • Oh W, DeLong R, Anusavice KJ. Factors affecting enamel andceramic wear: a literature review. J Prosthet Dent 2002;87:451-9.
  • Morneburg TR, Proschel PA. Measurement of masticatory forces andimplant loads: a methodologic clinical study. Int J Prosthodont2002;15:20-7.
  • Mitov G, Heintze SD, Walz S, Woll K, Muecklich F, Pospiech P.Wear behavior of dental Y-TZP ceramic against natural enamel afterdifferent finishing procedures. Dental Mater 2012;28:909-18.
  • McLean JW. Evolution of dental ceramics in the twentieth century. JProsthet Dent 2001;85:61-6.
  • Manicone PF, Rossi Iommetti P, Raffaelli L. An overview of zirconiaceramics: basic properties and clinical applications. J Dent2007;35:819-26.
  • Krejci I, Mueller E, Lutz F. Effects of thermocycling and occlusal24force on adhesive composite crowns. J Dent Res 1994;73:1228-32.
  • Krejci I, Lutz F, Reimer M, Heinzmann J. Wear of ceramic inlays,their enamel antagonists, and luting cements. J Prosthet Dent1993;69:425-30.
  • Kim M, Oh S, Kim J, Ju S, Seo D, Jun S, et al. Wear evaluationof the human enamel opposing different Y-TZP dental ceramics and otherporcelains. J Dent 2012;40:979-88.
  • Kadokawa A, Suzuki S, Tanaka T. Wear evaluation of porcelainopposing gold, composite resin, and enamel. J Prosthet Dent2006;96:258-65.
  • Jung Y, Lee J, Choi Y, Ahn J, Shin S, Huh J. A study on thein-vitro wear of the natural tooth structure by opposing zirconia or dental22porcelain. J Adv Prosthodont 2010;2:111-5.
  • Janyavula S, Lawson N, Cakir D, Beck P, Ramp LC, Burgess JO.The wear of polished and glazed zirconia against enamel. J Prosthet Dent2013;109:22-9.
  • Jang G, Kim H, Choe H, Son M. Fracture strength and mechanismof dental ceramic crown with zirconia thickness. Procedia Engineering2011;10:1556-60.
  • Jagger D, Harrison A. An in vitro investigation into the wear effects23of unglazed, glazed, and polished porcelain on human enamel. J ProsthetDent 1994;72:320-3.
  • Jacobi R, Shillingburg Jr HT, Duncanson Jr MG. A comparison ofthe abrasiveness of six ceramic surfaces and gold. J Prosthet Dent1991;66:303-9.
  • Hudson JD, Goldstein GR, Georgescu M. Enamel wear caused bythree different restorative materials. J Prosthet Dent 1995;74:647-54.
  • Helkimo E, Carlsson GE, Helkimo M. Bite force and state ofdentition. ActaOdontologica 1977;35:297-303.
  • Heintze S, Cavalleri A, Forjanic M, Zellweger G, Rousson V. Wearof ceramic and antagonist?A systematic evaluation of influencing factorsin vitro. Dental Mater 2008;24:433-49.
  • Harry A. Long. Monolithic zirconia crowns and bridges. InsideDentistry 2012;8:60-5.
  • Gibbs CH, Mahan PE, Lundeen HC, Brehnan K, Walsh EK,Holbrook WB. Occlusal forces during chewing and swallowing asmeasured by sound transmission. J Prosthet Dent 1981;46:443-9.
  • Elmaria A, Goldstein G, Vijayaraghavan T, Legeros RZ, HittelmanEL. An evaluation of wear when enamel is opposed by various ceramicmaterials and gold. J Prosthet Dent 2006;96:345-53.
  • Conrad HJ, Seong W, Pesun IJ. Current ceramic materials and systemswith clinical recommendations: a systematic review. J Prosthet Dent2007;98:389-404.
  • Christensen RP, Ploeger BJ. A clinical comparison of zirconia, metaland alumina fixed-prosthesis frameworks veneered with layered or pressedceramic: a three-year report. J Am Dent Assoc 2010;141:1317-29.
  • Christensen GJ. Porcelain-fused-to-metal versus zirconia-based ceramicrestorations. J Am Dent Assoc 2009140:1036-9.
  • Christensen G. PFM vs. zirconia restorations?how are theycomparing clinically. Clinicians Report 2008;1:1-2.
  • Chevalier J. What future for zirconia as a biomaterial? Biomaterials2006;27:535-43.
  • Blatz MB. Long-term clinical success of all-ceramic posteriorrestorations. Quintessence Int 2002;33:415-26.
  • Att W, Stamouli K, Gerds T, Rudolf Strub J. Fracture resistance ofdifferent zirconium dioxide three-unit all-ceramic fixed partial dentures.Acta Odontologica 2007;65:14-21.21
  • Ashkanani HM, Raigrodski AJ, Flinn BD, Heindl H, Mancl LA.Flexural and shear strengths of ZrO2 and a high-noble alloy bonded totheir corresponding porcelains. J Prosthet Dent 2008;100:274-84.
  • Anderson DJ. Measurement of stress in mastication. I. J Dent Res1956;35:664-70.
  • Albashaireh ZS, Ghazal M, Kern M. Two-body wear of differentceramic materials opposed to zirconia ceramic. J Prosthet Dent2010;104:105-13.
  • Abreu, Rogerio Alexandre Modesto de, Pereira MD, Furtado F, PradoGPR, Junior WM, Ferreira LM. Masticatory efficiency and bite force inindividuals with normal occlusion. Arch Oral Biol 2014;59:1065-74.
  • ?1. Holm C, Tidehag P, Tillberg A, Molin M. Longevity and quality ofFPDs: a retrospective study of restorations 30, 20, and 10 years afterinsertion. Int J Prosthodont 2003;16:283-9.